Highlights
- KU Leuven's SOLVOMET Group developed a precise method to measure cobalt salt dissolution using microcalorimetry and OLI Systems modeling software.
- Increasing methanesulfonic acid concentration reduced cobalt solubility roughly 300-fold, from 3.0 mol/L in water to 0.0100 mol/L at 80% MSA.
- The model performed reliably up to 80% acid concentration but was tested only on lab solutions, not real battery waste streams.
- Cobalt and nickel behave similarly in solution, making separation difficult and limiting direct industrial application without further testing.
- Researchers call for trials with mixed metals and actual recycling materials before claiming commercial-scale benefits.